How long does it take to repair PCB board oxidation?

by

2 Answers

+2 votes
 
Best answer

PCB board surface oxidation takes 1 to 2 days to repair.

After the PCB board surface is oxidized, the oxidized surface of the inner copper foil can be reduced with an alkaline solution containing dimethylborane as the main component. The reduced metallic copper can enhance acid resistance and improve adhesion; use a pH value of 3 Treat the copper surface whiskers with ~3.5 sodium thiosulfate reducing solution, acid leaching and passivation, and use ESCA to form a coating layer of copper and cuprous oxide mixture; use 1~2% hydrogen peroxide, 9~20% inorganic acid, 0.5 A mixture of ~2.5% tetraamine-based cationic surfactant, 0.1~1% corrosion inhibitor and 0.05~1% hydrogen peroxide stabilizer is used to treat the copper surface of the inner layer before laminating. The chemical tin plating process is used as the inner layer. The covering layer on the copper foil surface of the laminate.

by (32.4k points)
selected by
+1 vote

The time it takes to repair PCB board oxidation depends on the degree of oxidation and the repair method. If you use alcohol or thinner to wipe, soak the alcohol or thinner in a pure cotton cloth and gently wipe the oxidized part until the oxide is removed. This process may take several minutes to dozens of minutes. If a special cleaner is used, it may take anywhere from a few minutes to a few hours, depending on the situation.

If the PCB board is severely oxidized, more complex processing is required.

For example, use sodium thiosulfate reducing solution with a pH value of 3--3.5 to treat copper surface whiskers, acid leaching and passivation, and use ESCA to form a coating layer of a mixture of copper and cuprous oxide, or use 1-2% hydrogen peroxide. A mixture of 9-20% inorganic acid, 0.5-2.5% tetraamine-based cationic surfactant, 0.1-1% corrosion inhibitor and 0.05-1% hydrogen peroxide stabilizer is used to treat the copper surface of the inner layer plate before proceeding with the lamination process, etc. , these processes can take anywhere from hours to days.

Therefore, the time to repair PCB board oxidation depends on the degree of oxidation and the repair method, and the specific time needs to be determined based on the actual situation.

by (4.9k points)

Related questions

+2 votes
1 answer 41 views
41 views asked Nov 15, 2023 by PCB-Assembly-Factory (4.9k points)
+1 vote
1 answer 55 views
+1 vote
1 answer 37 views
37 views asked Nov 15, 2023 by PCB Design Company (26.6k points)
+1 vote
1 answer 48 views
+1 vote
1 answer 34 views
+1 vote
2 answers 37 views
+1 vote
1 answer 46 views
46 views asked Nov 19, 2023 by PCB European (26.3k points)
+1 vote
1 answer 42 views
+2 votes
1 answer 38 views
+1 vote
6 answers 86 views
+1 vote
1 answer 42 views
+1 vote
1 answer 48 views
+1 vote
1 answer 25 views
25 views asked Nov 9, 2023 by PCBManufactures (12.1k points)
+1 vote
1 answer 46 views
0 votes
1 answer 34 views
+1 vote
2 answers 37 views
+1 vote
1 answer 41 views
41 views asked Nov 22, 2023 by PCB-Assembly-China (32.4k points)
+1 vote
1 answer 45 views
45 views asked Nov 17, 2023 by PCB European (26.3k points)
+1 vote
3 answers 36 views
+1 vote
1 answer 32 views
+1 vote
2 answers 45 views
+1 vote
2 answers 42 views
...